PPS resin / Polyphenylene sulfide
Specifications
| Test item | Test condition | Test method | Test result | Unit |
| Physical properties | ||||
| Density | ASTM D792 | 1.8 | g/cm3 | |
| Molding shrinkage | ASTM D955 | 0.2-0.4 | % | |
| The ash content of coal | ASTM D2117 | 40 | % | |
| Tensile strength | 23°C,DAM | ASTM D638 | 140 | Mpa |
| Tensile elongation | 23°C,DAM | ASTM D638 | 6 | % |
| Flexural strength | 23°C,DAM | ASTM D790 | 220 | Mpa |
| Flexural modulus | 23°C,DAM | ASTM D790 | 12500 | Mpa |
| Notched Izod impact(1/8") | 23°C,DAM | ASTM D256 | 7 | KJ/m2 |
| Thermal properties | ||||
| Deflection temperature | 1.82Mpa | ASTM D648 | 260 | °C |
| Flammability | UL 94 | V-0 | — | |
| Machining parameters | ||||
| Drying temperature | — | 130-140 | °C | |
| Drying time | — | 3 | hr | |
| Processing temperature | — | 290-330 | °C | |
| Remarks | 40% Glass fiber reinforced | |||